Abstract
Metal nanoparticles have been used in the past to coat mild steel against corrosion due to
their outstanding mechanical and corrosion resistance properties. However, metal
nanoparticles when used to coat mild steel without solid support or host matrix have
shown some deficiencies such as micro cracking and pull-out of coatings from their
substrates because of their inherent high surface energy which tend to make them coalesce
to one another. Therefore, it is essential to trap these nanoparticles on a solid support when
used for coating to help them stay away from each other for improved protection
efficiency of nanomaterial coatings. This investigation was carried out on the development
of zinc-aluminum-titanium (Zn–Al–Ti) nanocomposite supported on biowaste based
activated carbon for coating of mild steel AISI 1015. Preparation of activated carbon from
groundnut shell with percentage carbon yield of 50.04% was undertaken by chemical
activation process, using ZnCl
2
as activating agent at optimized process conditions of 600
°C, 1.32 hours and 3, representing the activation temperature, activation time and
impregnation ratio respectively. A quadratic model was developed to correlate the
activation process parameters to the response (percentage yield) and it was observed that
the activation temperature with F-value of 2413.99 had the most significant effect on the
yield among the other process variables. Zn–Al-Ti metal nanocomposites supported
groundnut shell activated carbon (GSAC) coatings were developed by hosting the metal
nanoparticles on the GSAC, starting with Zn metal nanoparticles at three different mixture
ratios of 75:25 %wt, 50:50 %wt. and 25:75 %wt. The GSAC/Zn-Al-Ti sample formulated
at mixture ratio of 50:50 %wt. which gave the least average crystallite size of 35.24 nm
was then loaded into epoxy resin at four different ratios of 1:1, 2:1, 3:1 and 4:1 and coated
on mild steel. Porosity and micro hardness tests were carried out on the coatings. The least
percentage volume of porosity of 0.5% was achieved with the 2:1 ratio coating while the
maximum micro hardness value of 157 HV was recorded with the 4:1 ratio coating.
Optimum resistance to the corrosion of mild steel coupon in 1M HCl was achieved using
ratio 2:1, having recorded the least charge transfer resistance (R
ct
) of 42.51 KΩcm
and
protection efficiency of 98.73%.