<link rel="stylesheet" href="styles.f3b1fba60ec7970c.css">
FUT Minna Institutional RepositoryFederal University of Technology, Minna

Effects of Palm Leaf Ash and Palm Kernel Fibre on Properties of Compressed Laterite Earth Brick

dc.contributor.authorJude, Kolo
dc.contributor.authorEgwe, Christopher O.
dc.contributor.authorMohammed, Bala M.
dc.date.accessioned2023-07-02T02:00:45Z
dc.date.available2023-07-02T02:00:45Z
dc.date.issued2022
dc.descriptionA comparison of the properties of compressed laterite earth brick (CLEB) stabilized with palm leaf ash (PKA) and palm kernel fiber (KPF)en_US
dc.description.abstractThis study was designed to compare the effects of the properties of compressed laterite earth brick (CLEB) stabilized with palm leaf ash (PKA) and palm kernel fiber (KPF). The study was carried out in Building Technology Department, Federal Polytechnic Bida, Niger State. Bricks of 222×110×70 were produced using manual pressed machine where nine bricks each were stabilized with palm kernel fiber for 1%, 2%, and 3%. Also 9 bricks each were stabilized with palm leaf ash for each percent 5%, 10% and 15%. The materials used were Palm Kernel Fiber, Palm Leaf Ash laterite soil, and water. The abrasion resistance test and water penetration test were carried out. The findings revealed that the water penetration rate for the CLEB bricks stabilized with PKF recorded average penetration rate of 10.18 at 1%, 11.52 at 2% and 12.19 at 3%. Only 3% produced higher penetration rate while CLEB stabilized with PLA recorded average water penetration rate of 11.58 at 5%, 10.63 at 10%, and 11.27 at 15%. All were in conformity with NBRRI specification of 12.5%. The abrasion resistance of the 28 day CLEB stabilized with PKF recorded average abrasion of 1.40 at 1%, 1.28 at 2% and 3.68 at 3%. All result were conformity with the NBBRI specification of 6.9. While the abrasion esistance of the 28 day CLEB stabilized with PLA recorded average abrasion of 2.39 at 5%, 2.22 at 10% and 2.32 at 15% which were in conformity with the NBBRI specification of 6.9. Based on the findings of the study, it was concluded that the CLEB stabilized with palm kernel fiber at 1% and 2% are in conformity with NBRRI specification of compressive strength, water absorption rate and abrasion resistance. While compressed laterite bricks stabilized with palm leaf ash should be improve to conform to NBRRI specification.en_US
dc.description.sponsorshipSelfen_US
dc.identifier.citationJude, k., Egwe, C. O. & Mohammed, B. M. (2022)en_US
dc.identifier.issn2822-1737
dc.identifier.urihttp://repository.futminna.edu.ng:8080/jspui/handle/123456789/19253
dc.language.isoenen_US
dc.publisherJournal of Sustainability and Environmental Managementen_US
dc.relation.ispartofseriesVolume 1;Number 2
dc.subjectAbrasion resistance testen_US
dc.subjectBuilding materialen_US
dc.subjectEarth bricken_US
dc.subjectPalmen_US
dc.subjectWater penetration testen_US
dc.titleEffects of Palm Leaf Ash and Palm Kernel Fibre on Properties of Compressed Laterite Earth Bricken_US
dc.title.alternativeJournal of Sustainability and Environmental Managementen_US
dc.typeArticleen_US

Files

Original bundle

Now showing 1 - 1 of 1
Loading...
Thumbnail Image
Name:
Effects of Palm Leaf Ash.pdf
Size:
671.82 KB
Format:
Adobe Portable Document Format
Description:
A comparison of the effects of palm-leaf ash and palm kernel fibre

License bundle

Now showing 1 - 1 of 1
Loading...
Thumbnail Image
Name:
license.txt
Size:
1.71 KB
Format:
Item-specific license agreed upon to submission
Description: