Abstract
The mechanical properties of pipelines particularly those in marine
environments are influenced by corrosion activity of seawater throughout
their service lives. The degree to which these properties are influenced in
seawater compared to those exposed to air needs to be better
understood. In this study, the chemical composition of API X70 pipeline
steel plate, microstructure and mechanical properties of the welded joints
of same steel plates exposed to ambient air and seawater respectively
were investigated. It was found that the base metal consisted of
manganese (0.51wt% Mn), low carbon content (0.051 wt% C) and small
quantities of alloying elements such as vanadium (0.021wt% V),
molybdenum (0.118 wt% Mo), chromium (0.240 wt% Cr), copper (0.002
wt% Cu), and a carbon equivalent (CE IIW) of 0.38. Scanning Electron
Microscope (SEM) showed that the microstructure of base metal sample
has large grains formed in packets which have certain crystallographic
orientation but contain submicron grains arranged in a chaotic
interlocking manner. The tensile tests performed using a UNITED type
universal testing machine confirmed that the yield strength of the base
metal was 573.045MPa which conforms to API standard for X70 steel pipe.
The manual metal arc (MMA) welding technique was applied to produce
the welded joints. For the welded joints exposed to ambient air at room
temperature, the yield strength was 680.624MPa while the compressive
strength was 1500.2MPa, and the impact energy at -10°C was 112.68J. Air
tests referred to tests conducted in the laboratory at room temperature.
For the welded joints exposed to seawater for 12 weeks, the yield
strength was 609.154MPa while the compressive strength was
1219.34MPa, and the impact energy at -10°C was 61.48J. The above
results for air and seawater exposures were used to determine the
environmental reduction factors of the two environments. Hardness tests
conducted using Vickers hardness tester revealed variations in hardness
across the base metal, the HAZ and the weld, with the weld having the
highest average Vicker’s hardness value (223.8HV) followed by the base
metal (217.3HV) and the HAZ had the least (214.5HV)