Evaluation of some Combustion properties of Rice Husk Briquettes Produced at Varying Binder Concentrations from a Modified Block Briquetting Machine
Loading...
Date
Journal Title
Journal ISSN
Volume Title
Publisher
Direct Research Journal of Agriculture and Food Science
DOI
Abstract
Some combustion properties of rice husk briquettes
produced at varying binder concentrations from a modified
block briquetting machine that was designed and fabricated
in the Federal University of Technology Minna, Niger State,
Nigeria, were assessed with a view to ascertaining the best
binder concentration that produced the best briquettes in
terms of their combustibility. 10 kg of rice husk was
collected from Onyx rice mill, Bida, Niger State Nigeria.
They were manually cleaned to remove minor rice bran
particles and other impurities using sieve of hole size 3 mm
diameter. The rice husk were dried in the sun to 5% and
mixed with five different concentrations: 10 g, 20 g, 30 g, 40
g and 50 g and mixed uniformly. The resultant aggregates
were used to produce briquettes and sun dried for 3 days at
an average daily temperature of 32°C to a moisture content
of 5%. The process was replicated three times and their
combustion properties: percentage volatile matter, ash
contents, fixed carbon and heating values were evaluated.
The briquettes with lower starch concentration, 10% and
20 % had higher and similar volatile matter value of
72.00±0.01 d and 73.20±0.00 e respectively while the volatile
matter percentage reduce with increase in starch
concentration value from 68.49±0.04c to 57.14±0.01 a at
30% and 50%. Ash content values of the briquettes
produced increased from 9.73±0.00a at 10% binder
concentration to 22.15±0.00e at 50%.Fixed carbon percent
reduced from 18.27±0.01 b to 16.59±0.01 a at 10% and 20%
binder concentration levels and increased from 16.59±0.01 a
at 20% to 20.71±0.02 e at 50% binder concentration, while
heating value of briquettes reduced with increase in binder
concentration from 30.39±0.01 e MJ/kg to 26.25±0.00a
MJ/kg at 10% and 50% binder concentrations respectively.