Publisher: Bayero University, Kano
Abstract: LiSn2(PO4)3 of composition LiSn1.85Ti0.15(PO4)3 with NASICON structure was prepared by solid-state synthesis. XRD results show the formation of stable phase material of rhombohedral structure with the R3 ̅c space group. Traces of unreacted SnO2 and minor impurity of SnP2O7 were detected. Impedance and dielectric study in the microwave range show conductivity enhancement in bulk and grain boundary. The room temperature ionic conductivity is 4.74x10-5 S/cm and the conductivity at 740 K is 2.37x10-3 S/cm. The highest value of dielectric constant ε' obtained is 2000 and the lowest value is 500. Imaginary modulus vs temperature plot indicates the presence of temperature relaxation in the material. The plot of relaxation frequency at different temperatures was used to calculate the activation energy which was found to be 0.23 eV. These imply that the material could be applied as solid electrolyte at high temperatures.
Description: open access
URI: http://repository.futminna.edu.ng:8080/jspui/handle/123456789/11530
ISSN: 1597-9342
Appears in Collections:Physics

Files in This Item:
File Description SizeFormat 
BUK V8, N1. 2017 2nd (2).pdfhard copy17.54 MBAdobe PDFView/Open


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.